Welding rods
1.4430 DIN 8556: SG X 2 Cr Ni Mo 19 12 Welding of stainless, cold-strength and austenitic steels. For operating temperatures up to 400 °C.
1.4430 DIN 8556: SG X 2 Cr Ni Mo 19 12 Welding of stainless, cold-strength and austenitic steels. For operating temperatures up to 400 °C.
1.4430 DIN 8556: SG X 2 Cr Ni Mo 19 12 Welding of stainless, cold-strength and austenitic steels. For operating temperatures up to 400 °C.
1.4551 DIN 8556: SG X 5 Cr Ni 19 9 TIG or MIG / MAG welding of austenitic stainless steels Not for use in high-sulfur medium. For operating temperatures of up to 400 °C, scale resistant up to + 800 °C Delivered in carton quantities (1 or 3 packs)
1.4551 DIN 8556: SG X 5 Cr Ni 19 9 TIG or MIG / MAG welding of austenitic stainless steels Not for use in high-sulfur medium. For operating temperatures of up to 400 °C, scale resistant up to + 800 °C Delivered in carton quantities (1 or 3 packs)
1.4551 DIN 8556: SG X 5 Cr Ni 19 9 TIG or MIG / MAG welding of austenitic stainless steels Not for use in high-sulfur medium. For operating temperatures of up to 400 °C, scale resistant up to + 800 °C Delivered in carton quantities (1 or 3 packs)
1.4551 DIN 8556: SG X 5 Cr Ni 19 9 TIG or MIG / MAG welding of austenitic stainless steels Not for use in high-sulfur medium. For operating temperatures of up to 400 °C, scale resistant up to + 800 °C Delivered in carton quantities (1 or 3 packs)
1.4551 DIN 8556: SG X 5 Cr Ni 19 9 TIG or MIG / MAG welding of austenitic stainless steels Not for use in high-sulfur medium. For operating temperatures of up to 400 °C, scale resistant up to + 800 °C Delivered in carton quantities (1 or 3 packs)
1.4576 DIN 8556: SG X 2 Cr Ni Mo 19 12 Due to the addition of niobium, this steel has high strength and high resistance to intergranular corrosion.
1.4576 DIN 8556: SG X 2 Cr Ni Mo 19 12 Due to the addition of niobium, this steel has high strength and high resistance to intergranular corrosion.
1.4576 DIN 8556: SG X 2 Cr Ni Mo 19 12 Due to the addition of niobium, this steel has high strength and high resistance to intergranular corrosion.
1.4576 DIN 8556: SG X 2 Cr Ni Mo 19 12 Due to the addition of niobium, this steel has high strength and high resistance to intergranular corrosion.
1.4576 DIN 8556: SG X 2 Cr Ni Mo 19 12 Due to the addition of niobium, this steel has high strength and high resistance to intergranular corrosion.
1.4842 DIN 8556: SG X 12 Cr Ni 25 20 Welding of heat-resistant austenitic steels. The steel can be used in air up to approx. 1100 °C. Scale resistant up to 1100 °C.
1.4842 DIN 8556: SG X 12 Cr Ni 25 20 Welding of heat-resistant austenitic steels. The steel can be used in air up to approx. 1100 °C. Scale resistant up to 1100 °C.
1.4842 DIN 8556: SG X 12 Cr Ni 25 20 Welding of heat-resistant austenitic steels. The steel can be used in air up to approx. 1100 °C. Scale resistant up to 1100 °C.
1.4842 DIN 8556: SG X 12 Cr Ni 25 20 Welding of heat-resistant austenitic steels. The steel can be used in air up to approx. 1100 °C. Scale resistant up to 1100 °C.
1.4842 DIN 8556: SG X 12 Cr Ni 25 20 Welding of heat-resistant austenitic steels. The steel can be used in air up to approx. 1100 °C. Scale resistant up to 1100 °C.
Bonding and surfacing on stainless and acid-resistant Cr and Cr-Ni steels. Not for use in high-sulfur medium Operating temperatures from -196 °C to 350 °C Delivered in carton quantities (1 or 3 packs)